    Quote Originally Posted by bluesman7 View Post
    I was about to reply with the opposite. (I guess I sill am). My impression has always been that these colors were an in house code that varied from warehouse to warehouse, or mill to mill, possibly changing with heat number. I really don't know though. Maybe you and Substance can compare spark tests, since he has a bunch of known steels.
    Victor, thanks for posting on this. The reason I said universal is because there was a reference to a standardized color coding system chart that I found on the web 2 days ago but who knows what standards the MFG's use?
    bluesman7 likes this.
    Randolph Tuttle, a SRP Mentor for residents of Minnesota & western Wisconsin

  2. #22
    Heat it and beat it Bruno's Avatar
    Join Date
    Nov 2006
    Location
    Belgium
    Posts
    15,130
    Thanked: 5229
    Blog Entries
    10

    Default

    My O2 is dark blue at the end.
    Geezer likes this.
    Til shade is gone, til water is gone, Into the shadow with teeth bared, screaming defiance with the last breath.
    To spit in Sightblinder’s eye on the Last Day

  3. #23
    Hones & Honing randydance062449's Avatar
    Join Date
    May 2005
    Location
    Saint Paul, Minnesota, United States
    Posts
    7,973
    Thanked: 2204
    Blog Entries
    1

    Default

    Uddeholm steel color chart

    Name:  Uddeholm-color-chart.jpg
Views: 12926
Size:  71.5 KB

    Wordpress Color Codes | Coloring Anything
    Geezer and skipnord like this.
    Randolph Tuttle, a SRP Mentor for residents of Minnesota & western Wisconsin

  4. The Following 3 Users Say Thank You to randydance062449 For This Useful Post:

    Cangooner (06-11-2015), Substance (06-11-2015), Utopian (06-11-2015)

  5. #24
    Hones & Honing randydance062449's Avatar
    Join Date
    May 2005
    Location
    Saint Paul, Minnesota, United States
    Posts
    7,973
    Thanked: 2204
    Blog Entries
    1

    Default

    Victor, I just did some quick searching and I think your correct. Ok, so now I will try the spark testing and density methods.
    But no matter what the outcome I will still be using these steels as is !
    Substance and bluesman7 like this.
    Randolph Tuttle, a SRP Mentor for residents of Minnesota & western Wisconsin

  6. #25
    Senior Member blabbermouth Substance's Avatar
    Join Date
    Jun 2013
    Location
    Gladstone QLD AUSTRALIA
    Posts
    3,245
    Thanked: 804

    Default

    Quote Originally Posted by bluesman7 View Post
    I was about to reply with the opposite. (I guess I sill am). My impression has always been that these colors were an in house code that varied from warehouse to warehouse, or mill to mill, possibly changing with heat number. I really don't know though. Maybe you and Substance can compare spark tests, since he has a bunch of known steels.
    sounds good
    Saved,
    to shave another day.

  7. #26
    Senior Member
    Join Date
    Feb 2015
    Location
    Florida
    Posts
    507
    Thanked: 49

    Default

    All else aside, at worst, you have a lot of material for making good tools and such. Might have some folding knife blades hiding in the block of D2 if you are so inclined. My experience with US suppliers like Alro is that yellow on the end means 1018. The HRA(hot roll annealed) is probably 1018 too.

  8. The Following User Says Thank You to JDM61 For This Useful Post:

    Slawman (06-29-2015)

  9. #27
    Hones & Honing randydance062449's Avatar
    Join Date
    May 2005
    Location
    Saint Paul, Minnesota, United States
    Posts
    7,973
    Thanked: 2204
    Blog Entries
    1

    Default

    So far I have been working on putting together the parts for the post anvils. I now have 4 of the disc brake rotors for a base plus I have found the tubing to fit the various anvils and a guy who will do the cutting and welding ( Randy Stinar in Cannon Falls). They should be done in about 3 weeks.
    Randolph Tuttle, a SRP Mentor for residents of Minnesota & western Wisconsin

Page 3 of 3 FirstFirst 123

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •