Received this Hindostan in the post today from the u.k. Dimensions are 8" x 2 1/4" x 5/8". Out of flat on both major surfaces as well as being badly stained with iron oxide. In need of some serious work.
http://i1009.photobucket.com/albums/...psnp5auobz.jpg
http://i1009.photobucket.com/albums/...psmoxd9htj.jpg
After flattening on all sides with 220 sic powder on float glass.
http://i1009.photobucket.com/albums/...ps8jky9trh.jpg
Flattening on all sides with 320 grit W & D.
http://i1009.photobucket.com/albums/...pslqnojduc.jpg
End result after using 400 grit W & D.
http://i1009.photobucket.com/albums/...pserzpa7ni.jpg
Any of the members have experience using Hindostan Hones. Do the respond better to water or oil, what is the likely grit range, and would you classify them as a good quality hone. ??? Any background history on the Hindostan is also most welcome.
StewieS.
Victoria, Australia.