Has anyone used stropping compounds other than diamond or chrome oxide? Specificly. Cerium Oxide,
Linde, orTin Oxide for example.
-
06-29-2008, 05:54 AM #2
-
06-30-2008, 11:07 PM #3
- Join Date
- May 2005
- Location
- Saint Paul, Minnesota, United States
- Posts
- 8,023
- Blog Entries
- 1
Thanked: 2209None of those three, although the Linde is interesting.
Randolph Tuttle, a SRP Mentor for residents of Minnesota & western Wisconsin
-
10-06-2008, 04:16 AM #4
how about aluminum oxide?
alumina hones seem common.. same grit?
-
10-07-2008, 02:38 AM #5
Last week I made four bench strops from ½ birch ply with denim glued on one surface. I put chrome oxide, 1.8 boron carbide, rottenstone, and tin oxide on the last one tonight.
So far I have tried the chrome and the rottenstone, after coming of my yellow coticule. The rottenstone and chrome had very similar results. I will try the tin oxide later this week sometime.
I will break into my old telescope making boxes and dig up some cerium oxide and give it a try at a later date.
The linde abrasive seems like it would be a good choice.
I have read several old references to people stropping on bare aluminum. Aluminum forms an oxide very quickly on the surface I wonder how it would work. Have any of you tried it?
Charlie
-
10-07-2008, 02:43 AM #6
Rottenstone and chrome ox having similar results? Interesting. Are there varying grits of rottenstone? I bought a 1 pound box at a Rockler Woodworker store about a year ago and made a slurry with it on top of a Belgian Blue. Really terrible results. Very very gritty feeling.
Interesting idea about stropping on a polished aluminum plate. Very interesting.
Chris L"Blues fallin' down like hail." Robert Johnson