    Hi

    Some time ago I got a new coticule. La veinette, combo with manganese lines, cloudy blue hues. The stone is hard, very hard. The first slurry stone disintegrated, I wrote the mine itself and got another one. (let me say, the costumer services of Ardennes is first rate).

    The second slurry stone seemed to be tougher, but after a couple of months I notices that all the slurry comes from the slurry stone and not the hone itself, so I wrote again to Ardennes and they sent me 2 slurry stones, from the same la veinette vein both combo with BBW and tough as they come.

    My problem now is that I cannot make any slurry at all its like rubbing 2 pieces of glass.

    I do want to make the hone work, for touch ups its amazing, from hht 0, with dificult shaving to hht4 and amazing shave, it take only 100 laps on water. I would like to use it for the entire sharpening process.

    How can I make some slurry with such a hard stone?

    Thanks
    Last edited by Diegok; 11-28-2017 at 09:04 AM.
    Geezer likes this.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •