    hi guys can i have your advice and opinions on my honing progression m thinking about getting some 3m lapping film for finishing i already have hones i have diasharp 325 , 1k 4/8k norton combo , 6/10k combo 12k superstone.

    is it possible to go from 12k super stone to lapping film? then crock paste , leather strop

  2. #2
    Senior Member blabbermouth
    Join Date
    Apr 2012
    Location
    Diamond Bar, CA
    Posts
    6,553
    Thanked: 3215

    Default

    Yes, go from the 12k to 1um. 10- 15 laps usually. And then 10 laps on 1um with a sheet of copy paper under the film, to finish.

    If you use the copy paper, you won’t need Chrome Oxide and should have a very savable edge. You can touch up on 1um with paper when the edge starts to flag.

    Use the 1, 4. 8 and 12K progression leave the 6 & 10k out of the progression altogether, you do not need them.

    Do not buy diamond film, use Aluminum Oxide, or Silicon Carbide film from Thorlabs, (the best deal, with quality film). It works just as well, for literally 1/10 the cost of diamond film. Comes in 9X13 in sheets and you can cut into 4, 3 in pieces with a paper cutter.

    Get a glass 12 X 3 in glass tile from Lowes for about $4-5. You will have to lap it flat with 325 wet & dry or a diamond lapping plate, it laps easily and will make the film stick better.

    If you go from a 12k Super Stone you only need 1K film, .3 film is too harsh, for me and most folks.

    If you want a film progression, set the bevel on 1k and do a 5, 3,1um progression. Either way works. Film is excellent for hard, chip prone razors.

    A couple drops of Smith’s Honing Solution works well on the finish film.

  3. #3
    Senior Member
    Join Date
    Mar 2013
    Location
    Sydney Australia
    Posts
    173
    Thanked: 40

    Default

    Good advice given above!
    If you want to save a few dollars you could skip getting the glass plate. When I use lapping film I place it on top of the last stone I used (currently a Norton 8K), just rinse the stone of to remove ALL traces of grit, swarf and other debris.

  4. #4
    Member
    Join Date
    Jul 2012
    Posts
    53
    Thanked: 0

    Default

    Yes, go from the 12k to 1um
    is 1um 1 micron

  5. #5
    illegitimum non carborundum Utopian's Avatar
    Join Date
    Jan 2008
    Location
    Rochester, MN
    Posts
    11,544
    Thanked: 3795
    Blog Entries
    1

    Default

    Yes. 1um (micro-meter) is 1 micron, both of which are one millionth of a meter.

  6. #6
    Member
    Join Date
    Jul 2012
    Posts
    53
    Thanked: 0

    Default

    Quote Originally Posted by Utopian View Post
    Yes. 1um (micro-meter) is 1 micron, both of which are one millionth of a meter.
    ok great so i would like to apply the film to a hone so i dont need to buy a tile and flatten it so do i buy Aluminum oxide abrasive on 3 mil polyester film backing?
    or do i buy film with no backing?
    is 3m brand good enough quality or is there a better quality film?

    is there any benefit in progressing down to .3 or even 0.05?
    is Smith’s Honing Solution necessary/ do you need to water the film or use it dry?
    when doing the paper technique do you use damp paper?