When I hone on my Norton 4k and 8k using the pyramid method, I start to see what looks like steel particles on top of the hone where I am making my X stroke, and I was wondering if lapping the stones during the process is recommended. And if so, should I use my DMT stone to do it?


Also, what is "slurry"?