Bill - did you apply the cromox to the balsa with...
Bill - did you apply the cromox to the balsa with oil or any other medium? If so, that might be the answer right there.
I strop on a lot of different materials and view the edge under... -
04-02-2013, 05:40 PM
Thread: HHT better off 12k than crox
by Neil Miller- Replies
- 15
- Views
- 2,028
The shapton 16k glass stone is around 0.9 micron...
The shapton 16k glass stone is around 0.9 micron and the 30k shapton glass stone is around 0.4 micron, which is pretty close to good green chrome oxide - around 0.5 micron. So what you are really...