@Crackers Thanks for the tips mate - I will make sure to check out you tube for info on electrolysis
@tintin The aluminium plate is still being sourced - I may go with the hair dryer as I din't want to damage already delicate scales any more than necessary - more reading to be done yet
@Chevhead Thanks for the vote mate - and thanks for the inbox messages and tips.
@10Pups Nice tutorial video on the plating process --- maybe the wife will not be so happy about having sulphuric acid in the house with it being so nasty - I may try to ease her into it like I did with straight razors shaving
I'm about to start cleaning and sanding the blade and will be closely following the method used by 10Pups hopefully without cutting the fingers up. SWMBO gets upset when I do that. So it's going to be patience patience patience and don't rush anything.
Now it's off to make some sanding tools to help the process and minimize chances of Carpal Tunnel injury.