Quote Originally Posted by Chris L View Post
I tried to find info on the DMT website regarding the flatness of the Duosharp plates. Does anyone know whether they have any flatness claim like the metal DMT plates do?

Chris L
The plastic ones with the dimples are, from my recent recollection, rated at +- 0.003" vs the steel ones at +- 0.001". Still accurate enough... these are the outside extremes remember, not the average. The Bell curve dictates that most will have less variance, but some may be towards the outside limits... and depending on quality control, there is the chance some might not meet the standards... it happens to all manufacturers... even Shapton!

Regards

Kaptain "Poking fun where no one has poked before" Zero