Page 2 of 3 FirstFirst 123 LastLast
Results 11 to 20 of 23
Like Tree1Likes

Thread: Spill the beans, Jimmy!

  1. #11
    I used Nakayamas for my house mainaman's Avatar
    Join Date
    Aug 2009
    Location
    Des Moines
    Posts
    8,664
    Thanked: 2591
    Blog Entries
    1

    Default

    Quote Originally Posted by JimmyHAD View Post

    Thanks Stefan, reading So's stuff on his website I have the impression that he thinks it is advantageous to use the diamond plate for generating the slurry. For now I'm going to keep it simple and stick with that. I've noted various posts describing the naguras but I've never really studied the differences or which nagura might be suited to which hone. Something to look forward to in the future.
    Jimmy,
    I have experimented a lot with diamond plate and nagura and they are not mutually exclusive when we are talking about very hard and fine stones.
    The naguras pretty much are used as a progression after bevel set to bring the edge to the last polishing step done on the polishing stone.

    I was pretty skeptical of naguras initially but ever since I tried them I find them very very useful.
    Stefan

  2. #12
    Senior Member blabbermouth JimmyHAD's Avatar
    Join Date
    Feb 2008
    Posts
    32,564
    Thanked: 11042

    Default

    Quote Originally Posted by mainaman View Post
    Jimmy,
    I have experimented a lot with diamond plate and nagura and they are not mutually exclusive when we are talking about very hard and fine stones.
    The naguras pretty much are used as a progression after bevel set to bring the edge to the last polishing step done on the polishing stone.

    I was pretty skeptical of naguras initially but ever since I tried them I find them very very useful.
    Thanks Stefan. I expect that I will eventually dip my foot in that water. For now I'm taking baby steps with this J-nat stuff. If the economy ever bounces back in my lifetime and 'happy days are here again' I may broaden my horizons in the seemingly endless well of Japanese stones. For now I have to make do with what I've got.
    Be careful how you treat people on your way up, you may meet them again on your way back down.

  3. #13
    Senior Member
    Join Date
    Sep 2010
    Posts
    100
    Thanked: 25

    Default

    JUST MY OPINION

    If you're using slurry, I think it should always be a powdered version of the exact stone you're using, which means the nagura stone is either

    1. a piece broken off from your larger stone, or
    2. diamond

    There are dozens of different kinds of stones out there being sold as slurry or nagura stones. Unless you've been polishing Japanese swords for 20 years, I don't see how you could intelligently pick one to use with your particular finisher, much less a progression.

    JUST MY OPINION

  4. #14
    The Great & Powerful Oz onimaru55's Avatar
    Join Date
    May 2008
    Location
    Bodalla, NSW
    Posts
    15,606
    Thanked: 3748

    Default

    Quote Originally Posted by JimmyHAD View Post
    Thanks Stefan. I expect that I will eventually dip my foot in that water. For now I'm taking baby steps with this J-nat stuff. If the economy ever bounces back in my lifetime and 'happy days are here again' I may broaden my horizons in the seemingly endless well of Japanese stones. For now I have to make do with what I've got.
    Jimmy, if you hone with a progression of synthetics up to 8 k or even a bit higher, one good J-nat polisher is all you need... or maybe 2... or 3
    “The white gleam of swords, not the black ink of books, clears doubts and uncertainties and bleak outlooks.”

  5. The Following User Says Thank You to onimaru55 For This Useful Post:

    Disburden (01-06-2011)

  6. #15
    Senior Member blabbermouth JimmyHAD's Avatar
    Join Date
    Feb 2008
    Posts
    32,564
    Thanked: 11042

    Default

    Quote Originally Posted by wsfarrell View Post
    JUST MY OPINION

    If you're using slurry, I think it should always be a powdered version of the exact stone you're using, which means the nagura stone is either

    1. a piece broken off from your larger stone, or
    2. diamond

    There are dozens of different kinds of stones out there being sold as slurry or nagura stones. Unless you've been polishing Japanese swords for 20 years, I don't see how you could intelligently pick one to use with your particular finisher, much less a progression.
    Not just your opinion. I don't know if that is correct or not but I have read that So Yamashita (Japan Tool) prefers the diamond plate to create the slurry to avoid grit contamination. So says,

    "Secret MUST item for using hard natural stones. Nagura stones cannot be used for harder natural stones, nor on various Suita stones.

    The polishing parcticles of Nagura is larger than the particles of super fine finishing stones, and when the stone is hard, the Nagura's particle will scratch the bevel before they are ground to smaller size. Using diamond stone to create the initial slurry, you are getting the slurry that is made of the finishing stone itself. You'd be surprised how much better result you get by this technique.

    Also, when you use a Nagura on Suita stones, the coarse Nagura particles will get stuck in the Su (the holes in Suita stones) and will keep scratching the bevel, because these particles won't get ground to smaller sizes."

    Quote Originally Posted by onimaru55 View Post
    Jimmy, if you hone with a progression of synthetics up to 8 k or even a bit higher, one good J-nat polisher is all you need... or maybe 2... or 3
    Thanks Oz, that is exactly my routine. Right on about maybe 2 or 3 more .... or even more than that.
    Be careful how you treat people on your way up, you may meet them again on your way back down.

  7. #16
    The Great & Powerful Oz onimaru55's Avatar
    Join Date
    May 2008
    Location
    Bodalla, NSW
    Posts
    15,606
    Thanked: 3748

    Default

    Quote Originally Posted by JimmyHAD View Post
    Thanks Oz, that is exactly my routine. Right on about maybe 2 or 3 more .... or even more than that.
    I understand Jimmy. Each razor can be different so you need different stones
    “The white gleam of swords, not the black ink of books, clears doubts and uncertainties and bleak outlooks.”

  8. #17
    lz6
    lz6 is offline
    Senior Moderator lz6's Avatar
    Join Date
    Feb 2010
    Location
    California
    Posts
    4,833
    Thanked: 1841

    Default

    Nice Jimmy. I hope you have a great time with that beauty! Kindly keep us posted and add to my learning curve.
    Bob

    "God is a Havana smoker. I have seen his gray clouds" Gainsburg

  9. #18
    alx
    alx is offline
    Senior Member alx's Avatar
    Join Date
    Aug 2009
    Location
    Sonoma, California
    Posts
    418
    Thanked: 404

    Default

    Jimmy
    Looks like you got a winner there, you sure deliberated long enough and I admire your focus.

    Using a diamond plate (diamond nagura-DN or hon-nagura-HN) to raise a slurry is the fool proof method. A nagura stone is the more traditional approach in Japan although that is changing slowly. Using a DN will wear off grit faster and in my opinion this is the only drawback. Alx

  10. #19
    I Bleed Slurry Disburden's Avatar
    Join Date
    Feb 2009
    Location
    Carmel, NY
    Posts
    2,458
    Thanked: 545

    Default

    Quote Originally Posted by onimaru55 View Post
    You know they're hard when they challenge a diamond plate
    Fwiw, I have a Nakayama kiita that chewed up my credit card dmt 325 and wouldn't make slurry no matter how much I tried with it, just ended up with swarf on the stone.

  11. #20
    The Great & Powerful Oz onimaru55's Avatar
    Join Date
    May 2008
    Location
    Bodalla, NSW
    Posts
    15,606
    Thanked: 3748

    Default

    Quote Originally Posted by Disburden View Post
    Fwiw, I have a Nakayama kiita that chewed up my credit card dmt 325 and wouldn't make slurry no matter how much I tried with it, just ended up with swarf on the stone.
    I guess that's possible but how many strokes were you doing to slurry up ? I only ever use about 5-10 light strokes to create an almost invisible slurry with my Atoma 1200 for finishing.
    “The white gleam of swords, not the black ink of books, clears doubts and uncertainties and bleak outlooks.”