    When lapping a barber hone (and I have done about a dozen) I lap up to 1500 or 2000 grit and then apply a petroleoum product and let it soak for a week (I use vaseline on mine).
    How to lap a Barber hone. One of the better write ups on the subject done by our very own Modine.