Here are some photos of some more trials today with slurry on water. You can see with the slurry it finishes up as a hazy mirror. I finished this test piece with figure eights. Really a neat stone, wish I knew what the heck it was. I started this test with a 2,000 Shapton Pro then went straight to the new stone with an Atoma 400 slurry. This stone has really good feel on the water/slurry, I really like it. Took about 150 laps IIRC to remove every last one of the Shapton 2,000 scratches. It goes much faster if I start out at a 5,000 or 8,000 finish. I'm a little leery of trying to finish a razor on slurry though as I've never done it before.