View Poll Results: Which Combo do you use

Voters
162. You may not vote on this poll
  • 1k, 4k/8k, 12k, 16k, CRO2

    46 28.40%
  • BBW, Coticule

    28 17.28%
  • Lapping Film

    6 3.70%
  • 1k, BBW/Coticule, CRO2

    16 9.88%
  • Other, Explain please.

    76 46.91%
Multiple Choice Poll.
Results 1 to 10 of 91
Like Tree1Likes

Thread: The Hone stone Poll

Threaded View

  1. #30
    Beaker bevansmw's Avatar
    Join Date
    Feb 2008
    Location
    Hawaii
    Posts
    376
    Thanked: 35

    Default

    I use 1k, 4k, 8k and 16k shapton followed by powdered .5 micron chromium oxide on a 2" leather strop and about 50 laps linen and 100 leather on the regular strop.

    I've been thinking about replacing the 16k shapton with a japanese natural hone and getting a thin belgian coticule stone for warped blades, something like 1"x8" combo coticule. Above is what I use though.