I've been using JNATs for the past couple of months and love them as we'll. I was taught that you should not finish on plain water like a coticule. My understanding is that the slurry/swarf break down and create the finer and finer progression in and of itself. By going to straight water, again, my understanding, that you're actually going backwards with regards to refinement of the edge.