Results 1 to 10 of 32
Thread: How do you lap your stones?
-
02-16-2015, 12:22 AM #1
How do you lap your stones?
I've read articles and watched videos on all kinds of lapping methods. Lapping stones, diamond hones and flat tiles with wet/dry sandpaper are just a few of the examples. I'm curious what methods people are using and why. I know what has worked for me but am wondering if I can up my game.
Pete <:'}"Life is short, Break the Rules. Forgive quickly, Kiss Slowly,
Love truly, Laugh uncontrollably, And never regret ANYTHING
That makes you smile." - Mark Twain
-
02-16-2015, 12:33 AM #2
- Join Date
- Dec 2012
- Location
- Long Island NY
- Posts
- 1,378
Thanked: 177Ive used dmts, atomas and wet/dry. Recently got some sic powder and use that on a lapping plate. Im tired of spending money on another diamond plate. My atoma 140 used carefully is toast after one year. I mean it still works, but its toast compared to what it was. Spend 10 or 15 bucks on silicon carbide powder and a $5 granite tile from home depot and your good. You may want to use some wet dry to smooth them out depending on what your stone is. 140 grit is kinda of rough. You can get it in grit up to 1200 i think. But my 140 gets them flat fast and thats what I want.
-
The Following User Says Thank You to bill3152 For This Useful Post:
petercp4e (02-16-2015)
-
02-16-2015, 01:24 AM #3
- Join Date
- Feb 2013
- Location
- Haida Gwaii, British Columbia, Canada
- Posts
- 14,432
Thanked: 4826I do a fair amount of lapping. I lap coming off of a wet saw using a DMT lapping plate. I put a 1/2" thick rubber mat in the bottom of a sink or tub and put the lapping plate on top of that. Enough water to cover an inch over the top of the plate and lap away. I likely do more lapping than the average person due to the rockhound habit I have developed. It works well, however I have a plan to work on a larger motorized lapping system and it will likely utilize silicon carbide grit and a hard plate, most likely AR plate. The question that comes to mind is how much lapping does the average person do. Not likely enough to wear out a good lapping plate if used under water or under running water. They are not that much money and can be obtained from a lot of places, many of the wet shaving shops have them as well as and so does Lee Valley.
It's not what you know, it's who you take fishing!
-
The Following User Says Thank You to RezDog For This Useful Post:
petercp4e (02-16-2015)
-
02-16-2015, 01:40 AM #4
- Join Date
- Dec 2012
- Location
- Long Island NY
- Posts
- 1,378
Thanked: 177Yes I agree but even with light use the plates ''grit'' drops off drastically. With sic powder, its constantly refeshed. Faster cheaper and better imo. I wish someone told me this years ago. And a 12 x12 tile is a big surface so it goes fast. Use what you need and done.
-
The Following User Says Thank You to bill3152 For This Useful Post:
petercp4e (02-16-2015)
-
02-16-2015, 06:00 AM #5
- Join Date
- Sep 2013
- Location
- NW Indiana
- Posts
- 1,060
Thanked: 246Yes SiC loose grit is the way to go. I use it for all but the softest stones. Using it for the brunt of flattening work saves wear and tear on the diamond plates - which I still use on some stones such as Shaptons, and also for raising slurry on some natural finishers.
-
The Following User Says Thank You to eKretz For This Useful Post:
petercp4e (02-16-2015)
-
02-16-2015, 06:35 AM #6
- Join Date
- Jun 2012
- Location
- Land of the long white cloud
- Posts
- 2,946
Thanked: 580I have been using the three stone method if they are reasonably flat to start with, seems to work well on synthetics, and some naturals.
Into this house we're born, into this world we're thrown ~ Jim Morrison
-
The Following User Says Thank You to Grazor For This Useful Post:
petercp4e (02-16-2015)
-
02-16-2015, 09:55 PM #7
I usually just lap everything with my dmt 325. But it did wear out quite quickly, so I now use some wet dry sand paper.. Does the trick.. I'll try Bills sic powder method soon enough.. I don't hone often enough .. And the stones I have don't require lapping that often my choseras suehiros.. And a few jnat finishers along with my goto stone of the coticule or apache
-
The Following User Says Thank You to Airportcopper For This Useful Post:
petercp4e (02-16-2015)
-
02-17-2015, 02:54 AM #8
I just have a small DMT C about 1" by 4". I do very long light strokes and paid about 20 bucks for it. Cheaper then a lapping plate if you don't have a lot of stones to lap. That's another option for ya.
-
The Following User Says Thank You to s0litarys0ldier For This Useful Post:
petercp4e (02-17-2015)
-
02-17-2015, 02:59 AM #9
I use the Diamond plate under water as shown by Lynn Abrams. It seems to work great. I know there are other methods out there but that seems to work for me.
-
The Following User Says Thank You to rhensley For This Useful Post:
petercp4e (02-17-2015)
-
02-17-2015, 10:00 AM #10
- Join Date
- Feb 2015
- Location
- Canada
- Posts
- 5
Thanked: 2I use a Norton lapping stone that I keep flat with a DMT D6C, the DMT is a little small and it gets sticky unless the stones are being lapped under running water. A DMT D8C is more expensive than the two combined, but it works great also.
-
The Following User Says Thank You to IllegalMonk For This Useful Post: