Quote Originally Posted by RusenBG View Post
Ive been playng with the stone and is very god and fine one
make some slurry and after 7 - 8 K levell begin working on a thicker slurry and after 30 strokes make a quick dilution or dilucot - diluthur As you make the slurry more dilueted you also use less and less presure
in the end use plain watter for few strokes and with ultra light presure
Works very well every time
if you gett the blue - green stone , witckh is green wellow on the one side and the slurry is a good blue green stone
i think you will be very pleased with the results from this stone
gave amazing edges

Yes I got the blue/green one you were selling on etsy. It did leave an amazingly smooth edge. I quite enjoy the stone. It will remain my first and last thuringian. I think every man should own at least one thuringian in his honing kit.