07-09-2008, 12:02 AM #1
It was about 20 - 25 minutes or so each, I was lapping the right side the clear face of it and I was using a 1k shapton. I lapped four, so it took about 1 hr for two each time I lapped them.
-
07-09-2008, 12:54 AM #2
- Join Date
- Oct 2005
- Location
- Winnipeg Manitoba Canada
- Posts
- 1,333
Thanked: 351Uhh... sorry, but that explanation did not clear things up for me.... There is a clear glass side and a white ceramic side to the Glass Shaptons... It is the white side that is the honing surface, the other "clear" side is only the glass base and you can see the identification marks through it as in the grit mesh and micron size.
If you were lapping the white side of the hone, I cannot help but think that if you spent that much time on one hone, you must have accidentally used the wrong DMT plate or there is something terribly wrong with your DMT such as virtually no diamond grit. For me it was a matter of a few minutes with a almost instant white slurry being developed as I lapped the hones. The Shapton 2000 grit took the longest, my Shapton 16000 grit took the least amount of time which is to be expected as the diamonds have better access to the binder as the finer hones have smaller sized grit.
Regards
Christian"Aw nuts, now I can't remember what I forgot!" --- Kaptain "Champion of lost causes" Zero
-
07-09-2008, 01:57 AM #3
lol
So I had always thought the side you could see the identifcation marks through was the side you honed on. Well I suppose my base is perfectly flat now.
Guess I'll give it another go, I thought the white side was the base.
Suppose if I had read the back of the 16k's package that came in cardboard I'd of seen that, the other three came in black boxes.Last edited by bevansmw; 07-09-2008 at 02:14 AM.
-
07-09-2008, 02:18 AM #4
whew, now you can sharpen up some sh_teel much more easily
-
07-09-2008, 02:27 AM #5
- Join Date
- Oct 2005
- Location
- Winnipeg Manitoba Canada
- Posts
- 1,333
Thanked: 351Honestly, that's quite an understandable mistake.... after all, they did name them "Glass Hones", didn't they? Glad we got that sorted out and I'm confident you'll find things going much better this time.
Regards
Christian"Aw nuts, now I can't remember what I forgot!" --- Kaptain "Champion of lost causes" Zero
-
07-09-2008, 09:45 PM #6
I assumed prior to purchasing my Shapton ceramic stones and at that point only seeing pictures, that the honing surface was the glass surface. In my mind, I assumed you'd hone on the side that indicated the grit size, etc. So +1....don't feel bad about making the mistake of lapping the wrong side of these stones.
Chris L"Blues fallin' down like hail." Robert Johnson
"Aw, Pretty Boy, can't you show me nuthin but surrender?" Patti Smith
-
07-10-2008, 11:41 PM #7
I was fortunate and had seen the shaptons in use before deciding to buy so i already knew the "secret"
as for lapping them... i used the gdlp... on a base in my sink with a trickle of cool water splashing down.
500, 1k, 2k, 3k, 4k, 6k, 8k, 16k, 30k.... took 65 minutes all together, marking them each twice and lapping smooth. the worst stones were the 6k and 1k, the easiest the 8k and 30k. all except the 6k were high on just the ends the 6k had a high spot near the middle as well.
I lapped the 200 on a d8c took about 5 minutes.
Yes i liked the knifeforums group buy!Be just and fear not.