See:

ASTM D2256 Thread and Yarn Tensile Strength Test

For the ASTM test method for ultimate strength of thread/yarn. This is a starting point for ideas, with the razor introduced as a new feature.

Note that this test has a typical 10% relative standard deviation of ultimate force (to fracture). Typical deformation rates used are 0.8-4 mm/s.