11-01-2006, 03:15 AM
Thread: Thiers Issard grades
by Tony Miller- Replies
- 52
- Views
- 7,145
Joe, Those numbers would be inline with...
Joe,
Those numbers would be inline with hardening and annealing good steel and similar to what Mike has stated.
Tony -
10-27-2006, 01:43 AM
Thread: Thiers Issard grades
by Tony Miller- Replies
- 52
- Views
- 7,145
Joe, In normal forging of blades the steel will...
Joe,
In normal forging of blades the steel will be heated many times as it is shaped but it may not be at the initial solution temperature needed to start the real tempering process. Those first... -
10-26-2006, 06:54 PM
Thread: Thiers Issard grades
by Tony Miller- Replies
- 52
- Views
- 7,145
Joe, Although it melts at 850 deg. it can still...
Joe,
Although it melts at 850 deg. it can still be heated much higher than that. We use aluminum here for castings and although it melts at 1200 deg or so it can easily go far beyond that.
Tony -
10-20-2006, 12:41 AM
Thread: Thiers Issard grades
by Tony Miller- Replies
- 52
- Views
- 7,145
Most of the markings as joe said, such as Eagle,...
Most of the markings as joe said, such as Eagle, are used for different vendors so not two vendors in the same sales are (USA) will have the same production razors. On special editions...damascus,...