I wouldn't use pottery pigments on my razors...
I wouldn't use pottery pigments on my razors unless minimum mesh size of .5 micron is guaranteed.
Particle sizes are not always consistent & anything up to 40 micron could be present. -
06-12-2017, 02:01 AM
Thread: Maxing out Jnats
by onimaru55- Replies
- 29
- Views
- 2,865
Water or slurry finish is mostly dependant on the...
Water or slurry finish is mostly dependant on the stone.
The CrO is finer than Jnats especially as it is embedded into a soft substrate. As with using a .5 micron stone it is a quick n easy way... -
06-09-2017, 06:49 AM
Thread: Maxing out Jnats
by onimaru55- Replies
- 29
- Views
- 2,865
You wanna know the best way to max out a Jnat ? ...
You wanna know the best way to max out a Jnat ?
Do 5 strokes on a Gokumyo 20k to finish :roflmao