Results 1 to 10 of 10
Like Tree13Likes
  • 7 Post By tiddle
  • 1 Post By Splashone
  • 2 Post By RezDog
  • 1 Post By mainaman
  • 2 Post By cudarunner

Thread: Sandpaper progression -- Hand sanding

  1. #1
    Senior Member Siguy's Avatar
    Join Date
    Aug 2013
    Location
    Black Bear, NJ
    Posts
    1,672
    Thanked: 171

    Default Sandpaper progression -- Hand sanding

    Hey all.

    So I'm going to give my try hand sanding without the immediate use of the dremel.

    Can you share with me you prefered progressions of sandpaper grit?

    Regards,

  2. #2
    Senior Member tiddle's Avatar
    Join Date
    May 2012
    Location
    Oxford, Al
    Posts
    1,605
    Thanked: 407

    Default

    depends on what you're sanding. wood: 50 to knock of excess, 80 thorough shape, 120 to feather in overall shape, 180 to finish shaping, 220 to smooth and prep for finishing. g-10 and acrylic or phenolics, 80 to rough 120 to refine, 220 for final shape, 320 smooth, 600, 1200,2000 for polishing out deep scratches, buff with brown Tripoli diamond compound and chrome ox. metal is 220 dry, then wet, 400 dry then wet, 600 wet, 1200 wet, 2000 wet and buff for shine , or stop at 600 and buff with emory and blending bar for brighter satin or stop at emory and for dull satin. hope that helps!
    Mastering implies there is nothing more for you to learn of something... I prefer proficient enough to not totally screw it up.

  3. The Following 3 Users Say Thank You to tiddle For This Useful Post:

    rmagnus (11-27-2013), Seguragr (11-28-2013), Siguy (11-26-2013)

  4. #3
    Senior Member Siguy's Avatar
    Join Date
    Aug 2013
    Location
    Black Bear, NJ
    Posts
    1,672
    Thanked: 171

    Default

    @tiddle,
    That was an excellent post. I'm pretty new to this and have a follow easy question for you.

    When you say "then wet" for metal, are you actually sanding the blade *in* water or simply periodically wetting the sandpaper?

  5. #4
    Senior Member Splashone's Avatar
    Join Date
    Sep 2013
    Location
    Tucson, AZ
    Posts
    1,031
    Thanked: 176

    Default

    Keep the surface wet.
    Siguy likes this.

  6. #5
    Senior Member rmagnus's Avatar
    Join Date
    Sep 2013
    Location
    SoCal
    Posts
    248
    Thanked: 48

    Default

    tiddle nice guideline on sanding

  7. #6
    Senior Member souschefdude's Avatar
    Join Date
    Aug 2010
    Location
    Berks County PA
    Posts
    1,214
    Thanked: 180
    Blog Entries
    1

    Default

    Blade, visible rust, 400, 600, 800, 1000, 1500, 2000, ryobi white compound.
    Scales, 180 rough shape, 320 ,then same as blade.
    No hand sanding, double sticky back tape on a cork ina reversible drill.

  8. #7
    Senior Member blabbermouth RezDog's Avatar
    Join Date
    Feb 2013
    Location
    Haida Gwaii, British Columbia, Canada
    Posts
    14,439
    Thanked: 4827

    Default

    wet sanding on metal is often done with wd-40 or similar very light oil.
    gssixgun and traps38 like this.

  9. #8
    Senior Member robert2286's Avatar
    Join Date
    Oct 2013
    Location
    Albuquerque
    Posts
    508
    Thanked: 32

    Default Sandpaper progression -- Hand sanding

    I use wire brush first and then 280grit , 1000, 1500, 2000 basically 500 grit increments all the way to 12000 with micromesh! Then buffing wheel on a drill with white/red compounds ! And i only use water with it! Micromesh is reusable so it will last u a couple of restorations! If u get it... Make sure u ck the dimensions! First time i got the micromesh circles and they are smaller than a quarter! Lol! Get the 2x2 squares
    Last edited by robert2286; 11-28-2013 at 03:22 PM.

  10. #9
    I used Nakayamas for my house mainaman's Avatar
    Join Date
    Aug 2009
    Location
    Des Moines
    Posts
    8,664
    Thanked: 2591
    Blog Entries
    1

    Default

    I start with 400 or 600 depending on the situation.
    I use slurry froma natural Japanese stone, but you can also add slurry from synthetic 1k. Adding the slurry makes the sanding effect very even as the sandpaper wears out. Keep using the same piece of sand paper till you are done with that stage. After that, you move to next grit of sand paper, usually 1500 grit. I use 2k slurry with that grit. After those stpes you should have very fine scratches barely visible after you polish with metal polish such as Mothers, Flitz etc.

    This one I did hand polish using the described method, no visible scratches on the blade after.

    Last edited by mainaman; 11-28-2013 at 03:56 PM.
    WadePatton likes this.
    Stefan

  11. #10
    'with that said' cudarunner's Avatar
    Join Date
    Aug 2010
    Location
    Walla Walla in WA State USA
    Posts
    11,226
    Thanked: 4237

    Default

    While I ‘technically’ don’t ‘hand sand’ as I use a palm sander I’ve never used 220 wet and dry, if I have to go ‘low’ I use 320.

    I do think that it’s important especially to those who are new to remember that every blade doesn’t have to have a near mirror finish!! It’s sometimes good to leave a little of the Heritage and or Battle Scars!

    For instance:

    Before:

    Name:  Campbell's Razor Before 2.jpg
Views: 280
Size:  60.7 KB

    After:

    Name:  1 Campbell's Clean up.jpg
Views: 233
Size:  55.5 KB

    Before:

    Name:  003.jpg
Views: 235
Size:  74.3 KB

    After:

    Name:  First After Pic.jpg
Views: 232
Size:  78.4 KB

    And of course what Glen did for my Great Grandfather's W&B:

    Before:

    Name:  WB 1.jpg
Views: 215
Size:  43.8 KB

    After:

    Name:  WB 8.jpg
Views: 238
Size:  34.0 KB

    All of the razors are good shavers, they still have a little 'character' to remind that they have survived abuse, neglect and time!!

    Enjoy the journey, it's a long strange trip!!
    Luis and Razorfeld like this.
    Our house is as Neil left it- an Aladdins cave of 'stuff'.

    Kim X

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •