I was once told by a plating outfit when the electroplating solution is basically played out and it's full of all sorts of garbage since they don't want to throw away any gold they use it down to the last drop so they decide what the cutoff is and lower the prices and you get a dirty low K plate that isn't very durable at all.

And that is basically gold wash.