    Default

    I only use slurry with Jnats and can't say I find differences. For me with that type of stone there is none. I am talking about hard J-nats that do not release slurry on their own.
    Wolfpack34 likes this.
    Stefan

  2. The Following User Says Thank You to mainaman For This Useful Post:

    gssixgun (12-01-2015)

  3. #2
    Senior Member Wolfpack34's Avatar
    Join Date
    Apr 2011
    Location
    California
    Posts
    1,596
    Thanked: 865

    Default

    Quote Originally Posted by mainaman View Post
    I only use slurry with Jnats and can't say I find differences. For me with that type of stone there is none. I am talking about hard J-nats that do not release slurry on their own.
    I am obviously out of the 'loop' having never heard of 'slurry-dulling' before, and having no idea on how to explain the term???

    Name:  confused.jpg
Views: 704
Size:  45.4 KB

    Having said that I agree with Stefan...except I also use slurry with Coticules. My Escher's are water only finishers (Usually), and I use oil on the CF's and LI's and the Arks.
    engine46 and Aaron71 like this.
    Lupus Cohors - Appellant Mors !

  4. The Following User Says Thank You to Wolfpack34 For This Useful Post:

    gssixgun (12-01-2015)

  5. #3
    I used Nakayamas for my house mainaman's Avatar
    Join Date
    Aug 2009
    Location
    Des Moines
    Posts
    8,664
    Thanked: 2591
    Blog Entries
    1

    Default

    Quote Originally Posted by Wolfpack34 View Post
    I am obviously out of the 'loop' having never heard of 'slurry-dulling' before, and having no idea on how to explain the term???

    Name:  confused.jpg
Views: 704
Size:  45.4 KB

    Having said that I agree with Stefan...except I also use slurry with Coticules. My Escher's are water only finishers (Usually), and I use oil on the CF's and LI's and the Arks.
    I think there are too many "experts" out there that like to invent new things so they can stand out of the crowd of honers that is swarming the internets. I do not think there is such thing as slurry dulling but may be someone can come here with facts and prove me wrong.
    Wolfpack34, jfk742 and jnats like this.
    Stefan

  6. The Following 2 Users Say Thank You to mainaman For This Useful Post:

    gssixgun (12-01-2015), Wolfpack34 (12-01-2015)

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •