I was wondering given that the 12k stone are reportadly so hard they might abrade the ceramic shapton equally and keep it in optimum shape. I have a x course DMT for lapping but have not needed it yet for my 16000 shapton. I have gotten by so far with rubing the swarf off with run water and finger pressure.