    Default MuellerThuringian as a finisher stone?

    I am currently looking for a finishing stone and i did find this: Olivia's handgemachte Naturseifen

    Or would the chines 12k be a better choice?

    best regards

  2. #2
    Hones & Honing randydance062449's Avatar
    Join Date
    May 2005
    Location
    Saint Paul, Minnesota, United States
    Posts
    8,023
    Thanked: 2209
    Blog Entries
    1

    Default

    My vote would be for the Ch12K. It is a slow cutter ( about 100 laps) but pretty predictable in the results. I like them so much I purchased a second as a backup.

    Just my $.02,
    Randolph Tuttle, a SRP Mentor for residents of Minnesota & western Wisconsin

  3. #3
    aka shooter74743 ScottGoodman's Avatar
    Join Date
    Sep 2009
    Location
    SE Oklahoma/NE Texas
    Posts
    7,285
    Thanked: 1936
    Blog Entries
    4

    Default

    I ordered a couple a while back and have opened one up, lapped it, and used it. Long story short, I would not recommend it as a finisher. I have not at this time determined where it falls in the "grit" scale, but what I do know is that it will deteriorate a shave ready razor that shaves smoothly to scratchy. From those couple razors I tested it on, I know that my shapton 8k is a smoother shaver than the finish I received from that stone. Under 100x it does NOT polish the edge. I did this honing starting with a slurry using the provided slurry stone and would keep adding water until it was only the stone and water. I've put it in my "soaker" tub and haven't gone back to it to try and "learn" what it has to offer.

    Please keep in mind that these are natural stones and there could be a chance I just got a "not so good" meuller stone. I'll open up the other one one of these days when I get back to honing a few razors.

    At this time, I would recommend the chinese stone. I do know for a fact that my chinese stones are more finishers than my muellers...actually by a long shot.

    If you go for a chinese stone, get a larger one as they are slow stones and the more stone the better. I purchased both of mine from Woodworking Plans & Tools | Fine Woodworking Project & Supplies at Woodcraft
    Hope this helps,
    Scott
    Southeastern Oklahoma/Northeastern Texas helper. Please don't hesitate to contact me.
    Thank you and God Bless, Scott

  4. #4
    Member
    Join Date
    Jan 2010
    Posts
    76
    Thanked: 10

    Default

    Thanks for you answers. It seems like i will go for the C12K , Unfatherly I live in europe so i will have to look for the c12k inside the union. If anyone have any place to recommend except the polish lad on ebay it would be most welcome

  5. #5
    I Bleed Slurry Disburden's Avatar
    Join Date
    Feb 2009
    Location
    Carmel, NY
    Posts
    2,458
    Thanked: 545

    Default

    It is not like an old thuringian stone or Escher at all. I bought one a few years ago and it sits in a drawer somewhere not being used.


    I would say it is 6K.

  6. #6
    aka shooter74743 ScottGoodman's Avatar
    Join Date
    Sep 2009
    Location
    SE Oklahoma/NE Texas
    Posts
    7,285
    Thanked: 1936
    Blog Entries
    4

    Default

    You may have better luck finding a thuringian, they are more common over there on the other side of the pond...
    Southeastern Oklahoma/Northeastern Texas helper. Please don't hesitate to contact me.
    Thank you and God Bless, Scott

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •