Results 11 to 13 of 13
-
03-01-2012, 03:25 AM #11
Don't use the DMT EE 8k as a lapping plate; slurry will remove the plating that holds the diamonds onto the plate (likewise, to the E 1200). Use a DMT C 325 or 120 for lapping and rinse it regularly.
I'm also an ME/EE and prefer fast results for the same reasons. Exactly what I use since about January 2009, if you change crox to black Dovo ~1micro. The crox I still use about 5-10% of the time, superb stuff.
The set of mini-hone stones that can actually fit in the pocked and are basically maintenance free would consist of: DMT W4E, DMT W4EE, Swaty stone.
Then I actually found this post from a guy that seems to be happy:
http://straightrazorpalace.com/hone-...-000-mesh.html
I think I will give it a try to see how this solution can be and evaluate time, maintenance, consistent results etc etc etc.
Note that this would just be a side experiment for people like me: Stressed, lack of time, no space, no time for maintenance, that just want to be able to set low/medium straights to be shave ready in a consistent and acceptable solution.
This is not a replacement for a decent honing system with proper stones, that in the end is the best solution. Its just an experiment as proof of concept.
Any feedback on the 3-stone mini hone system is more then welcome! All hones regardless of material should fit in a human hand, thats my requirement aswell
Search for some of Seraphim's posts (here and at B&B), since he does something similar; only he often finishes up on a surface plate with coated plastic/paper abrasives.
-
03-02-2012, 10:20 AM #12
get a second swaty, and rub em together for slurry
-
03-02-2012, 06:20 PM #13
Ill order chosera 1k soon it comes with a slurry. I need to sell of someday of my heljestrand and Anton bergs first. I have to many...
Glen Do i need a 3 or 5 kr naniwa aswell? I Do have a cheaper 3/8k combo from Taidea