Results 1 to 10 of 16
Threaded View
-
12-18-2013, 11:13 AM #9
- Join Date
- Dec 2012
- Location
- Long Island NY
- Posts
- 1,378
Thanked: 177That's a great combination IMO. The 20 k really produces. It had the same softish feel at first as the naniwa, but after using for a while and lapping it, it gets real hard and doesn't need lapping often. They give you a slurry stone with it, its 1k,4k. This is for resurfacing the stone and removing swarf, it works very well. Good luck with it.