    Default Grit of Aloxite Hone by The Carborundum Co?

    Would anyone happen to know the grit of an aloxite hone that I have that's manufactured by The Carborundum Company?
    Here's a picture of it:
    http://countryjoe.bizland.com/store/...azor-hone.html

  2. #2
    Senior Member
    Join Date
    Mar 2007
    Posts
    281
    Thanked: 0

    Default

    Would anyone have any idea how to lap an aloxite/aluminum oxide hone? It's incredibly hard, ~9 on the Mohs scale. Any suggestions would be appreciated.

  3. #3
    Member AFDavis11's Avatar
    Join Date
    May 2005
    Location
    Virginia
    Posts
    5,726
    Thanked: 1486

    Default

    I lap barber hones together, your is probably in the neighborhood of 9k. I apply lather to my barber hones to get them as slow as possible, but they are good wet too. Have fun.

    BTW, barber hones are often flat enough to hone without lapping. They are harder than ordinary water hones.

  4. #4
    Senior Member
    Join Date
    Mar 2007
    Posts
    281
    Thanked: 0

    Default

    Thanks for your response. Mine was completely flat, but it had pock marks in it. The only way I could get rid of them was by using a 3M pad since it ground sandpaper off all together. The pockmarks are gone, but do you have any ideas on how I could restore it to its former glassy finish?

  5. #5
    Vitandi syslight's Avatar
    Join Date
    Jan 2007
    Location
    Scharie County, NY USA
    Posts
    2,761
    Thanked: 224

    Default i sense the cringing...

    I lapped an aloxite stone and an ole pike (norton) Krystalon on my notrton lapping stone... it took a good while but i eventoaully got them flat. It also took some time to clean the lapping stone afterwards.

    as far as getting that smooth shiny look / feel back just hone a few ebay specials and it will be back.
    Be just and fear not.

  6. #6
    Senior Member
    Join Date
    Mar 2007
    Posts
    281
    Thanked: 0

    Default

    Thanks, I'll see if I can get my hands on the flattening stone. Was your aloxite pretty aggressive? Mine puts a nice edge on a dull razor within about 5 round trip passes or so, but I kept getting somewhat mixed results with my razors due to the pock marks.

  7. #7
    Member AFDavis11's Avatar
    Join Date
    May 2005
    Location
    Virginia
    Posts
    5,726
    Thanked: 1486

    Default

    Wow, thats fast! I need to use shaving lather on every barber hone I've ever used to slow it down. Do you mean it refreshes the edge with 5-6 laps, thats normal. But it brings up a dull razor that fast?
    Last edited by AFDavis11; 03-03-2007 at 01:00 PM.

  8. #8
    Senior Member
    Join Date
    Mar 2007
    Posts
    281
    Thanked: 0

    Default

    Heh heh. Sorry, I meant that it refreshes a slightly dull edge within those passes to shaving sharp.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •