Page 1 of 2 12 LastLast
Results 1 to 10 of 13
  1. #1
    Senior Member Tuxedo7's Avatar
    Join Date
    Oct 2009
    Location
    Jacksonville, FL
    Posts
    161
    Thanked: 33

    Default Are all Henckels Friodur's Stainless???

    I've seen a few Friodur's without "no-stain" identified ... are these stainless/no-stain? Or are there some carbon steel Friodur's out there. I assume from the name that the freeze/cold treatment implied in the name (Friodur) that all Friodur's are Stainless, but want to confirm.

  2. #2
    < Banned User >
    Join Date
    Feb 2008
    Posts
    3,763
    Thanked: 735

    Default

    There are many Henckels razors out there that are neither Friodurs, nor stainless.

    But my understanding is that all Henckels Friodurs are stainless.

  3. The Following 2 Users Say Thank You to Seraphim For This Useful Post:

    cutter2001 (12-02-2009), Tuxedo7 (12-01-2009)

  4. #3
    Large Member ben.mid's Avatar
    Join Date
    Aug 2008
    Location
    Oxfordshire, England
    Posts
    3,096
    Thanked: 763

    Default

    Yep. I'm fairly confident they are. The Friodur was the stainless range.

  5. The Following User Says Thank You to ben.mid For This Useful Post:

    Tuxedo7 (12-01-2009)

  6. #4
    At this point in time... gssixgun's Avatar
    Join Date
    Jun 2007
    Location
    North Idaho Redoubt
    Posts
    27,026
    Thanked: 13245
    Blog Entries
    1

    Default

    I wasn't that positive on it, I thought that Friodur meant Frozen temper but the "no-stain" stamp were SS Frozen temper...

    I would like to know for sure though...

  7. The Following 2 Users Say Thank You to gssixgun For This Useful Post:

    cutter2001 (12-02-2009), Tuxedo7 (12-01-2009)

  8. #5
    Large Member ben.mid's Avatar
    Join Date
    Aug 2008
    Location
    Oxfordshire, England
    Posts
    3,096
    Thanked: 763

    Default

    Here's a page from the Zwilling site. It relates to knives, but i guess the principles are the same.
    They state.

    "Freezing to -70°C.
    Ice-hardening strengthens the corrosion resistance and thus protects better against rust."

    That's as much info as i could find.

  9. The Following User Says Thank You to ben.mid For This Useful Post:

    Tuxedo7 (12-01-2009)

  10. #6
    Senior Member matt321's Avatar
    Join Date
    Jul 2007
    Location
    United State of Texas
    Posts
    635
    Thanked: 139

    Default

    I read somewhere that cryo treatment for cutlery steel was mostly a stainless thing.
    Last edited by matt321; 11-26-2009 at 06:13 PM.

  11. #7
    Senior Member blabbermouth JimR's Avatar
    Join Date
    Dec 2008
    Location
    Japan
    Posts
    2,746
    Thanked: 1014
    Blog Entries
    2

    Default

    Well, I'm not sure about Friodurs but I had a Sub Cero, the Filarmonica cryo-treated blade I believe, that certainly wasn't VERY stainless, judging by all the stains that were on it (it was stored NEXT TO an Inox, which was pristine...). So maybe they did both, carbon and stainless?

  12. The Following User Says Thank You to JimR For This Useful Post:

    Tuxedo7 (12-01-2009)

  13. #8
    At this point in time... gssixgun's Avatar
    Join Date
    Jun 2007
    Location
    North Idaho Redoubt
    Posts
    27,026
    Thanked: 13245
    Blog Entries
    1

    Default

    Yeah I am pretty sure that "Frozen/Cyro/Sub Zero" doesn't just pertain to SS The DD Wonderedge is carbon too..... BUT that wasn't really the question here...

    I have seen Friodur stamps
    I have seen Friodur No-Stain stamps
    I have seen Friodur Inox stamps

    This is what give me a small element of doubt....

  14. The Following User Says Thank You to gssixgun For This Useful Post:

    Tuxedo7 (12-01-2009)

  15. #9
    Senior Member blabbermouth JimmyHAD's Avatar
    Join Date
    Feb 2008
    Posts
    32,564
    Thanked: 11042

    Default

    I'm clueless on this question. I can say that all of the Friodurs I've ever seen have been stainless but I am sure I haven't seen them all.
    Be careful how you treat people on your way up, you may meet them again on your way back down.

  16. The Following 2 Users Say Thank You to JimmyHAD For This Useful Post:

    cutter2001 (12-02-2009), Tuxedo7 (12-01-2009)

  17. #10
    Senior Member matt321's Avatar
    Join Date
    Jul 2007
    Location
    United State of Texas
    Posts
    635
    Thanked: 139

    Default

    Don't know much about this, but here is an example of what i had read:
    In most low-alloy steels, there is little or no difference achieved by cryo-treatment. This is because low-alloy steels do not retain austenite. Some bladesmiths indicate that if low-alloy steel has received good heat-treating, there will be nothing left for the cryogenic process to work with.
    Sword Forum Magazine - From the Forge - Cryogenics
    Last edited by matt321; 11-26-2009 at 06:39 PM.

  18. The Following User Says Thank You to matt321 For This Useful Post:

    Tuxedo7 (12-01-2009)

Page 1 of 2 12 LastLast

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •