    Quote Originally Posted by mainaman View Post
    I only use slurry with Jnats and can't say I find differences. For me with that type of stone there is none. I am talking about hard J-nats that do not release slurry on their own.
    I am obviously out of the 'loop' having never heard of 'slurry-dulling' before, and having no idea on how to explain the term???

    Name:  confused.jpg
Views: 691
Size:  45.4 KB

    Having said that I agree with Stefan...except I also use slurry with Coticules. My Escher's are water only finishers (Usually), and I use oil on the CF's and LI's and the Arks.
    engine46 and Aaron71 like this.
    Lupus Cohors - Appellant Mors !

  2. The Following User Says Thank You to Wolfpack34 For This Useful Post:

    gssixgun (12-01-2015)

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •