Results 31 to 40 of 45
Thread: DMT 8C or ATOMA?
-
12-05-2013, 11:53 PM #31
-
12-05-2013, 11:59 PM #32
I use my DMT8C for all of my stones, there is no negative effect using it on the Naniwa 12k,
some do prefer a finer finish on there finishers and I have lapped my 12k on 2k wet dry and have seen no difference in the finished product.
That being said I know some naturals will perform better with a glazing/glass finish
but then gents that really know the naturals will have to chime in as I am just getting started with natural stones.It is just Whisker Whacking
Relax and Enjoy!
-
The Following User Says Thank You to pfries For This Useful Post:
Ludvig (12-06-2013)
-
12-06-2013, 12:25 AM #33
-
12-06-2013, 12:42 AM #34
- Join Date
- Dec 2012
- Location
- Long Island NY
- Posts
- 1,378
Thanked: 177I have dmts and atomas. I have the 400 and 1200 atoma. I hardly use the 400. The 1200 I use all the time as I maintenance lap my hones, I don't wait for them to get out of shape, just to keep on top of them and I use them almost everyday. You may be better served using coarser wet dry for the time or two you need it and finish with the 1200 that you will use often. A 400 or 325 IMO is too rough for a 12k stone. I just got a few new Jnats and I use 60 grit wet dry to get them mostly flat before I will sacrifice an expensive diamond plate. Just something to think about. And the plates do not last forever.
-
12-06-2013, 12:42 AM #35
Hi there! I have the 400 Atoma and the 1200 as well as a DMT325 (well worn). For dressing, I would prefer to use the well worn DMT on my finishers (Shapton glass 16k and the other naturals) before I use the 400 Atoma. I believe the Atoma 1200 or the DMT325, dress the surface better on the 8k level and up, than the Atoma 400 does. But to be honest I have only tried the Atoma 400 up to the 8k Shapton glass only (to dress the surface) and I don't remember being any different on the final edge. But the lapping I have done on the turi, for example, with the 400 Atoma doesn't leave as smooth a surface as the Atoma 1200 does.
Somebody will have to comment on the 600. I think it could work, but I don't have one! The 400 is a stone eater, making all initial lapping a breeze that produce an even "smooth" flat surface. The 1200 shines in lapping already lapped surfaces or refreshing and dressing a stone for honing, specially finishers (8k and up).
If you want, you could use a new DMT325 for your initial 1k to 12k or 16 k lapping, follow by the Atoma 1200 to lap and dress stones from 4k up. I wouldn't use the Atoma 1200 for 1k lapping, IMO. Hope this helps! Double O
-
The Following User Says Thank You to Double0757 For This Useful Post:
Ludvig (12-06-2013)
-
12-06-2013, 12:49 AM #36
-
12-06-2013, 02:39 AM #37
-
12-06-2013, 04:01 AM #38
Would it be out of the question for you to buy 2 plates ?
I used a 1200 Atoma to lap as low as 800 King stone. It worked just fine but it did break in quickly & had I continued it might've broke down quickly too. it would be ideal to have the 400 as well but if you buy the 400 alone you could then use your stones to lap each other. e.g. flatten your 12k with the 400 Atoma then use your 8k to smooth the face of the 12k.The white gleam of swords, not the black ink of books, clears doubts and uncertainties and bleak outlooks.
-
-
12-06-2013, 04:27 AM #39
-
The Following User Says Thank You to edhewitt For This Useful Post:
Ludvig (12-06-2013)
-
12-06-2013, 02:23 PM #40
Ludvig
I mainly use the #600 Atoma for general stone dressing and flattening like when I am at my bench honing razors, and the #400 when I need to actually flattening a stone that has a dish shape or frown shape. I have the DMT, but the Atoma product to me feels a lot more like a tool in my had because of the heavy milled metal base plate.
So for average daily work with the #600 I find that the scratches it leaves on the stones can me minimalized with lighter pressure and by allowing the mud to remain as you lap instead of using it under running water.
Alex
-
The Following User Says Thank You to alx For This Useful Post: