Did these tonight. Got plenty more to go. Will give them a test shave in the morning.
Antoni Tadross 2798 Germany, TTC Clean shave Germany and a J.A. Helberg Skydds Marke Eskilstuna.It's just Sharpening, right?
Jerry...
-
08-03-2017, 12:55 AM #1802
- Join Date
- Mar 2015
- Location
- Indiana, Portland
- Posts
- 321
Thanked: 70I too like the Genco. I have three and they are all very good. I consider them some of the best buys in my collection.
-
08-04-2017, 11:36 PM #1803
A Bruno blade off the Norton India....
-
08-05-2017, 12:08 AM #1804
Nice!
Cheers, Steve
-
08-05-2017, 12:25 PM #1805
-
08-05-2017, 10:07 PM #1806
Honing last week sucked. I tried the Gok20k but was getting chippy edges even with jointing and going back to 8k. Next I tried the Ohzuku and the shave wasnt great. So when it all fails I go back to the green Nakayama, raised slurry with 1200 Atoma this time and worked all the way down to water.
This AM the shave was perfect with the 6/8 Dovo. Alum didn't sting a bit. I know that HHT is subjective but after stropping on the fire hose and then the Kanayama this razor is giving silent ones.
-
08-06-2017, 12:55 AM #1807
Just a thought. All the extra work after the 20k may have solved the problem rather than any one stone being the solution.
Slurry work on fast cutting Jnat finishers can often "heal" an edge especially after restorations where one can sometimes miss clearing up early stage bevel work.The white gleam of swords, not the black ink of books, clears doubts and uncertainties and bleak outlooks.
-
The Following User Says Thank You to onimaru55 For This Useful Post:
alex1921 (08-06-2017)
-
08-06-2017, 05:19 PM #1808
Testing a members pretty pretty coticule.
Mike
-
08-08-2017, 03:26 AM #1809
- Join Date
- Aug 2013
- Location
- Orangeville, Ontario
- Posts
- 8,449
- Blog Entries
- 1
Thanked: 4206Finished up some Japanese blades on some jnats.
A couple Saito creations, the SK3 and the Gloria, a Trade Mark, and a folding kami 'Hatori Deluxe' that seems to be made of very hard steel..
And also put my Riga to the Escher to clean up the edge a skosh.
Some very sharp edges, and a nice way to finish a long weekend.
Cheers men."Depression is just anger,, without the enthusiasm."
Steven Wright
https://mobro.co/michaelbolton65?mc=5
-
08-09-2017, 04:33 AM #1810
Two Harts just shy of 8/8" two layers of tape to give the edge strength
Shapton Pro 1k, 2k, 5k 8k and my unknown jnat
Jnat finish was dmt 1200 credit card slurry then tomo nagura slurry diluted to a few water only X strokes